InoK-MZ


InoK-MZ is a versatile inoculant with controlled amounts of Manganese, Zirconium and Barium. A highly potent inoculant with good fading resistance for both Gray and S.G.iron.

3-6 mm

3-6 mm

1-3 mm

1-3 mm

0.2-0.7 mm

0.2-0.7 mm

 

Chemical Analysis

% Si
% Zr
% Ba
% Mn
% Ca
% Al
% Fe
60-67
5-7
2.0-2.5
5-7
1.0-1.5
1.0-1.5
Balance

Application

Gray Iron

  • Rapid dissolution even at low temperature.
  • Very good chill reduction even in thin sections.
  • Good resistance to fading.
  • Promotes A type graphite in both thick and thin sections.

S.G.Iron

  • Dissolves fully even at low temperature.
  • Good increase in Nodule Count.
  • Good Fading Resistance.
  • Not suitable for fully ferritic S.G.irons.
Melting Point

1170-1250 °C.

Size Range 0.2-0.7 mm, 1-3 mm, 3-6 mm, 6-10 mm.
Addition
Ladle
Late Stream
Gray Iron
0.2-0.3 %
0.05-0.1 %
S.G.Iron
0.25-0.4 %
0.05-0.1 %
Packing 50 Kg, 1000 Kg – HDPE Bags
Storage If stored in low humidity environment in the same packing, product can be preserved for a long time.